Effect of microwave hybrid heat treatment on the microstructure and hardness of 3D printed Inconel 718 superalloy
- Post by: admin
- juillet 3, 2023
- No Comment
M. Sadeghifar, M. Javidikia, A. Loucif, M. Jahazi, V. Songmene
Journal of materials research and technology 24, 395-406