Effect of microwave hybrid heat treatment on the microstructure and hardness of 3D printed Inconel 718 superalloy

Effect of microwave hybrid heat treatment on the microstructure and hardness of 3D printed Inconel 718 superalloy

M. Sadeghifar, M. Javidikia, A. Loucif, M. Jahazi, V. Songmene
Journal of materials research and technology 24, 395-406